Technical Notes/Selection2026-11-19

Selecting Superalloys by Service Temperature: Three Boundaries at 650, 750 and 950 °C

"Superalloy" spans very different materials at 650 °C and 950 °C. Fix the service temperature, stress and atmosphere first, and the grade list usually narrows to two or three options.

Red-hot workpieces inside a superalloy heat-treatment furnace

The most common mistake in buying superalloys is asking for a grade before describing the service condition. The order should be reversed: temperature, stress, atmosphere and required life. Temperature is the hardest boundary, and engineering practice usually splits it into three bands.

Below 650 °C: economy first

In this band, load-carrying parts can start with iron-nickel age-hardening alloys. GH2132 (A286, UNS S66286) is the classic choice — strength and oxidation resistance are sufficient and cost is clearly lower than nickel grades. Fasteners, springs and discs use it extensively. Where relaxation resistance matters a little more, the move is to GH4145 (X-750).

650–950 °C: the nickel age-hardening divide

This is the home ground of GH4169 (Inconel 718) — highest yield strength among wrought nickel alloys below 650 °C, mature processing, wide supply. Above 650 °C for long times, 718 loses strength as γ″ coarsens into δ; the move is to GH4145, Nimonic 90, or solid-solution grades such as GH3044 and GH3039.

Above 950 °C: oxidation becomes the first criterion

At this temperature strength is no longer the only issue — oxide scaling and microstructural stability kill parts. Typical choices are solid-solution grades: GH536 (Hastelloy X), GH5188 (Haynes 188), 602CA and cobalt-based HS25 (L605). They are chosen not because they are strongest, but because they hold together without spalling.

A three-step rule

Check the temperature band, then whether the part is load-bearing over long times, then whether the atmosphere contains sulfur, chlorine or is strongly oxidizing. If any one crosses a boundary, move up a class. When in doubt, send us the service condition — narrowing to two or three candidates with reasons is faster than scanning grade tables.

This article is a general technical note on materials and processing; cited standards are public standard numbers. Specific grades, sizes and acceptance items are subject to the technical agreement confirmed by both parties.

LET'S MAKE IT WORK

Match the material to your service conditions.

Submit a technical requirement